Page 1 - SD 2507Cu
P. 1

PRODUCT DATA SHEET

                                    Corrosion Stainless Steel



             DUPLEX STAINLESS STEEL GRADE








                                                               +
                                      SD 2507Cu (UR 52N ) is a super duplex stainless steel with 25% Cr and a
                                      PREN  value  higher  than 40. The minimum guaranteed yield strength  is  550 MPa
                                      which  allows  the  designer  to  reduce  weight.  The  molybdenum  and  nitrogen
                                      additions  have  been  optimized  in  order  to  obtain  the  best  corrosion  resistance
                                      properties  even  for  heavy  plates.  High  nitrogen  content  improves  the  structure
                                      stability  particularly  in  HAZ.  Its  corrosion  resistance  is  much  better  than  UR
                                      B6/N08904 and roughly equivalent to 6 Mo super austenitic alloys.

                                      Copper  additions  increase  the  corrosion  resistance  properties,  particularly  in
                                      sulphuric acid media.

                                      SD  2507Cu  is  a  cost  efficient  grade  designed  for  offshore,  marine,  phosphoric
                                      acid, sulphuric acid applications... as well as pollution control equipments.




                                                                                 +
         STANDARDS                    SD 2507Cu........................................ UR 52N
                                      EURONORM .................................... 1. 4507 - X2 Cr Ni Mo Cu N 25.6.3
                                      AFNOR .............................................. Z3 CNDU 25.07 AZ
                                      ASTM. ........................................... UNS S32550/S32520



          CHEMICAL                           Typical values (Weight %)

          ANALYSIS                         C         Cr        Ni        Mo         N            Others
                                         < 0.030     25        6.5       3.5       0.25          Cu  1.5
                                                          PREN = [Cr %] + 3.3 [Mo %] + 16 [N %]  40


                                            Tensile properties - minimum values
         MECHANICAL                             Rp 0.2   Rp 1.0   Rm            YS 0.2%   YS 1.0%   UTS    El
                                                                                                           %
         PROPERTIES                      °C     MPa      MPa      MPa     °F     KSI      KSI     KSI     25
                                                          570
                                                                          68
                                                                   770
                                                 550
                                         20
                                                                                                  111
                                                                                  78
                                                                                          83
                                         100     485      500      700    212     70      72      102     25
                                         250     400      420      640    500     57      61       92     25
                                            Typical temperature range of use : -50°C/+ 270° C (-58°F /+518°F)
                                            For lower temperature applications, please contact us.
   1   2   3   4   5   6